Chap. xi.
Wrought Iron, not excited by a loadstone, draws iron.
F rom the ore, which is converted, or separated, partly into metal, partly into slag, by the intense heat of fires, iron is smelted in the first furnaces in a space of eight, ten, or twelve hours, and the metal flows away from the dross and useless matter, forming a large